Ключевые слова: Abies wood, Hydrogen peroxide, Kinetics, Optimization, Oxidative fractionation, TiO2 catalyst, Activation energy, Atmospheric pressure, Catalysts, Cellulose, Delignification, Enzyme kinetics, Kinetic theory, Numerical methods, Oxidation, Peroxides, Rate constants, Titanium dioxide, Experimental and numerical methods, First order equations, Kinetic study, Micro-crystalline cellulose, Optimal parameter, Temperature range, Wood
Аннотация: The kinetic study of abies wood delignification by H2O2 in the medium acetic acid–water was first carried out in the presence of TiO2 catalyst under mild conditions: temperatures 70–100 °C, atmospheric pressure. The oxidative delignification process is described satisfactory by the first order equation in all temperature range. TheПоказать полностьюrate constants varied between 0.80 and 12.3 ? 10?3 min?1 and the activation energy was near 81 ± 0.21 kJ mol?1. The optimal parameters of the delignification process, providing the effective fractionation of abies wood on microcrystalline cellulose and soluble lignin, were established by experimental and numerical methods. © 2016, Akademiai Kiado, Budapest, Hungary.
Журнал: Reaction Kinetics, Mechanisms and Catalysis
Выпуск журнала: Vol. 120, Is. 1
Номера страниц: 81-94